PRECISION FORM
2Pages

{{requestButtons}}

Catalog excerpts

PRECISION FORM - 1

PRECISION FORM Downgauging of sanitary ends using DR plate before bottom dead center bottom dead center Conventional Process - thinnning Precision Form Process - no thinnning

Open the catalog to page 1
PRECISION FORM - 2

AEROSOL BOTTOMS titans Haar Downgauging of pressure can bottoms using DR plateMATERIAL BUCKLE BURSTTHICKNESS PRESSURE PRESSURE in mm in bar in bar Remark: buckle pressure values are 50% higher than the accepted pressure values inside the cans at 50°C ALFONS HAAR MASCHINENBAU GMBH & CO. KG • Fangdieckstrasse 67 • D-22547 Hamburg • TEL +49 40 83391-0 • FAX +49 40 844910 INTERNET www.alfons-haar.de ♦ E-MAIL office@alfons-haar.de 2266872.2 Subject to alteration